+86 18002889642
info@new-silicone.com

Newsil — Silicone Rubber & Foam Manufacturer

Fluorosilicone Rubber Compound

+8618002889642
info@new-silicone.com

Fluorosilicone Rubber Compound

Fluorosilicone Rubber is a specialized elastomer that combines the properties of silicone rubber and fluorocarbon rubber. It is known for its exceptional resistance to fuels, oils, solvents, and extreme temperatures, making it suitable for demanding applications in aerospace, automotive, and industrial sectors.

Features

  1. Exceptional chemical resistance (fuels, oils, solvents, acids).
  2. Wide temperature range (-60°C to 200°C).
  3. Fuel and oil resistance (jet fuels, diesel, gasoline, hydraulic fluids).
  4. Weather and ozone resistance (UV, ozone, weathering).
  5. Good compression set resistance.
  6. Flame resistance (inherently flame-retardant).
  7. Low gas permeability.

Applications

  1. Aerospace: Fuel system seals, O-rings, hydraulic components.
  2. Automotive: Fuel injector seals, valve stem seals, engine gaskets.
  3. Oil and Gas: Downhole seals, refinery gaskets, chemical-resistant parts.
  4. Industrial: Chemical processing seals, machinery components.
  5. Electrical: Harsh environment seals, insulators.
  6. Medical/Food: Biocompatible seals, food-contact gaskets.
  7. Military: Fuel system seals, engine components.

Technical Index

Original Technical Index

Property Unit Test Method Typical Value
Hardness Shore A Shore A ASTM D-2240 50 
Tensile Strength MPa ASTM D-412 8.6 
Elongation at Break % ASTM D-412 345 
Specific Gravity g/cm3 ASTM D-792 1.42 
100% Tensile Strength MPa ASTM D-412 1.5 
Rebound % ASTM D2632 33 

Heating Aging, 72hrs@225℃

Property Unit Test Method Typical Value
Change in Hardness Shore A ASTM D-573
Change in tensile strength % ASTM D-573 -17 
Change in Elongation % ASTM D-573 -16 

Reference Fuel C 70 h at 23°C

Property Unit Test Method Typical Value
Change  in Hardness Shore A ASTM D-471 -4 
Change in tensile strength % ASTM D-471 -18 
Change in Elongation % ASTM D-471 -20 
Change in Volume % ASTM D-471 +18.5 

Fluid Resistance IRM 903 Oil 70 h at 150°C

Property Unit Test Method Typical Value
Change  in Hardness Shore A ASTM D-471 -2 
Change in tensile strength % ASTM D-471 -13 
Change in Elongation % ASTM D-471 -13 
Change in Volume % ASTM D-471 +3.9 

Fluid Resistance IRM 901 Oil 70 h at 150°C

Property Unit Test Method Typical Value
Change  in Hardness Shore A ASTM D-471
Change in tensile strength % ASTM D-471 -13 
Change in Elongation % ASTM D-471 -12 
Change in Volume % ASTM D-471 +1.2 

100℃×70h/ biodiesel 70 h at 100°C

Property Unit Test Method Typical Value
Change  in Hardness Shore A ASTM D-471 -4 
Change in tensile strength % ASTM D-471 -16 
Change in Elongation % ASTM D-471 -14 
Change in Volume % ASTM D-471 +5.7 

SAE 5W30engine oil 150℃×100h

Property Unit Test Method Typical Value
Change  in
Hardness
Shore A ASTM D-471 -1 
Change in tensile strength % ASTM D-471 -6 
Change in Elongation % ASTM D-471 -14 
Change in Volume % ASTM D-471 +2.2 

Compression Set, Aged0 168 hours @ 150℃

Property Unit Test Method Typical Value
6mm Buttons % ASTM D-395












Chat on WhatsApp